Schmelzpunkt
°C
|
oxidierende
Bedingungen
|
reduzierende
Bedingungen
|
Vakuum
|
Inertgas
|
| Al2O3 |
2053
|
1600
|
1600
|
1600
|
1600
|
| BN |
2700-3000*
|
1000
|
1800
|
1400
|
1800
|
| MoSi2 |
2030
|
1700-1900
|
1700-1900
|
1700-1900
|
1700-1900
|
| SiC |
2300
|
>1000
|
>1000
|
>1000
|
>1000
|
| Si3N4 |
1900*
|
1100
|
1850
|
1100
|
1850
|
| MgAl2O4 |
2120
|
1500
|
1500
|
1500
|
1500
|
| TiC |
3140
|
2000
|
2000
|
2000
|
2000
|
| TiN |
2950
|
500
|
1500
|
1500
|
1500
|
| Y2O3 |
2410
|
2200
|
1500
|
2200
|
2200
|
| ZrB2 |
3040
|
----
|
----
|
1800
|
1800
|
| ZrO2 |
2700
|
1900
|
1500
|
1900
|
1900
|
|